| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 175 - 220 °C | 347 - 428 °F | Average value: 189 °C Grade Count:26 |
|
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | |
|
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer
Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%...
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Average value: 208 °C Grade Count:8 |
|
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical ALPHALAC SG910 HIPS
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical ALPHALAC SG960 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical ALPHALAC SG970 HIPS
Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical HIPS 60HRI PS, Impact Modified
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical HIPS MI750L PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1045D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | |
|
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as..
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
|
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
|
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
|
|||
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection |
|
Lubrizol ESTANE® GP55DT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 55DT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | |
|
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | |
|
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA)
Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Nozzle Temperature | 185 - 220 °C | 365 - 428 °F | Injection |
|
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection |
|
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer
Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Nozzle Temperature | 175 - 220 °C | 347 - 428 °F | Average value: 205 °C Grade Count:6 |
|
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
|
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec..
|
|||
| Nozzle Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
|
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
|
|||