Polymer Property : Nozzle Temperature = 250 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Nozzle Temperature 250 °C
482 °F
NYCOA 2001 PA 6
high melt strength general extrusion and molding grade of nylon 6Information provided by NYCOA, Inc.
Nozzle Temperature 250 °C
482 °F
NYCOA 2012 Copolymer Nylon
easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc.
Nozzle Temperature 250 °C
482 °F
NYCOA 578 PA 6
very high viscosity molding & extrusion grade for tubing, pipes, film and tapesInformation provided by NYCOA, Inc.
Nozzle Temperature 250 - 260 °C
482 - 500 °F
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber
Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo..
Nozzle Temperature 250 - 304 °C
482 - 580 °F
Average value: 283 °C Grade Count:4
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Nozzle Temperature 250 - 295 °C
482 - 563 °F
Average value: 279 °C Grade Count:5
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7854 PBT, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Nozzle Temperature 250 - 260 °C
482 - 500 °F
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Nozzle Temperature 250 - 260 °C
482 - 500 °F
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7557 PBT, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour, self-lubricating, for highest tribologic needs.Low warpag..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Nozzle Temperature 250 - 270 °C
482 - 518 °F
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Nozzle Temperature 250 °C
482 °F
Tipco Tipcofil® AGM 602 - 10% Mineral & 20% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability
10% Mineral + 20% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Nozzle Temperature 250 - 270 °C
482 - 518 °F
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Nozzle Temperature 250 - 270 °C
482 - 518 °F
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Nozzle Temperature 250 - 270 °C
482 - 518 °F
Tisan TISLAMID® 66 UNR Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Nozzle Temperature 250 - 310 °C
482 - 590 °F
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Average value: 258 °C Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..