| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
PolyOne Nymax™ 1200 IL Natural Polyamide 66 (Nylon 66)
The Nymax® 1200 IL is an internally lubricated, unfilled nylon 6/6 designed for exceptional processing and mold release. This grade is intended primarily for injection molded applications where a g..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3/TF/20/BK Polyamide 6, with PTFE
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-7451 Polyamide 6, lubricant modified, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.dynamic stressReduced moment of inertia compared with metal parts.Be..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
|
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant
Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose
Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
|
|||
| Nozzle Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
|
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
|
LG Chemical LUMID GP2330BL PA66+GF33%, General Purpose
Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Radiator Tank, Reservoir)Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
|
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose
Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
|
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose
Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
|
LG Chemical LUMID SG2300B(W) PA66+GF30%, General Purpose, Good Surface
Feature: Injection Molding, PA66+GF30%, General Purpose, Good SurfaceApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 310 °C | 518 - 590 °F | |
|
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi..
|
|||
| Nozzle Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
|
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
|
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
LG Chemical LUPOY GP-1000 General Purpose Modified PC, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
LG Chemical LUPOY GP-1006F General Purpose Modified PC, Unreinforced, Weather Resistant, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai..
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
Unitika U-8000
U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than..
|
|||
| Nozzle Temperature | 270 - 310 °C | 518 - 590 °F | Average value: 290 °C Grade Count:3 |
|
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
|
|||