| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
PTS Tristar® PC-10FR-(18) 18 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hybrid B2025IU Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Nozzle Temperature | 260 - 271 °C | 500 - 520 °F | |
|
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Nozzle Temperature | 260 - 271 °C | 500 - 520 °F | |
|
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled
Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone
|
|||
| Nozzle Temperature | 260 - 271 °C | 500 - 520 °F | |
|
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled
Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone
|
|||
| Nozzle Temperature | 249 - 271 °C | 480 - 520 °F | |
|
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Mitsubishi Iupilon® H2000R 23 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend
Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 7901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 266 - 271 °C | 510 - 520 °F | |
|
Diamond Polymers ASA M-523
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Diamond Polymers ASA S319
Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Diamond Polymers ASA T-110
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 221 - 271 °C | 430 - 520 °F | |
|
Diamond Polymers ASA TW-20
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized
Data provided by Clariant Masterbatches
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 8901
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 266 - 271 °C | 510 - 520 °F | |
|
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | Average value: 254 °C Grade Count:5 |
|
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin
(discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
Diamond Polymers ABS/PC 9801
Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Nozzle Temperature | 238 - 271 °C | 460 - 520 °F | |
|
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
|
|||