| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 330 °C Grade Count:22 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301/XCF/30 N PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7153 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7932 PPS, linear, with aramid reinforcement and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8148 PPS, linear, with PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-7094 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-7796 Polyphthalamide, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-8261 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Nozzle Temperature | 320 - 330 °C | 608 - 626 °F | |
|
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
|
|||