| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 175 °C | 347 °F | |
|
Termopol Termoton® K2GA5050A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||
| Nozzle Temperature | 175 °C | 347 °F | |
|
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80/CF/10/BK Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80/TF/18/GY Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7666/GY Polyacetal-copolymer, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7713-NA Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7718 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8106 Polyacetal-copolymer, with carbon fiber, PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8162 Polyacetal-copolymer, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8222 Polyacetal-copolymer, with mineral filler, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8284 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8387/EM Polyacetal-copolymer, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, ..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8510 Polyacetal-copolymer, with mineral filler, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally..
|
|||
| Nozzle Temperature | 175 - 185 °C | 347 - 365 °F | Injection Molding |
|
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane
ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Huntsman AVALON® 85 ABX Thermoplastic Polyurethane
Introduction: AVALON 85 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABX is part of the AVALON Perform Range and offers a specially designed,..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
|
|||
| Nozzle Temperature | 175 - 200 °C | 347 - 392 °F | |
|
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
|
|||
| Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
|
Lubrizol Estane® T460A Thermoplastic Polyurethane
Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
|
|||
| Nozzle Temperature | 175 - 190 °C | 347 - 374 °F | |
|
Lubrizol Estane® T465A Thermoplastic Polyurethane
Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
|
|||
| Nozzle Temperature | 175 - 220 °C | 347 - 428 °F | Average value: 205 °C Grade Count:6 |
|
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
|
|||