| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber
Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
|
|||
| Nozzle Temperature | 225 - 280 °C | 437 - 536 °F | Average value: 246 °C Grade Count:4 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
|
|||
| Nozzle Temperature | 235 - 280 °C | 455 - 536 °F | Average value: 263 °C Grade Count:3 |
|
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-7281/PL/HI/BK Polyamide 6, with PTFE, toughness-modified
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
|
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant
Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose
Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical
|
|||
| Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
|
LG Chemical LUMID HI1202A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
|
LG Chemical LUPOY GN5001RFP PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch..
|
|||
| Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
|
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
|
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature
Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided..
|
|||
| Nozzle Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
|
LG Chemical LUPOY HP5004A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102..
|
|||
| Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
|
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
|
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
|
|||
| Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
|
LG Chemical LUPOY SR3108L PC, High Impact
Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Gromax CCP PET 9130-104 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..
|
|||
| Nozzle Temperature | 275 - 280 °C | 527 - 536 °F | |
|
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy
Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d..
|
|||
| Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
|
|||