| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
|
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
|
|||
| Nozzle Temperature | 245 - 290 °C | 473 - 554 °F | |
|
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte..
|
|||
| Nozzle Temperature | 177 - 290 °C | 351 - 554 °F | Average value: 225 °C Grade Count:5 |
|
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)
(Unverified Data**)
Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi..
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose
Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
|
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
|
LG Chemical LUMID HI2302A(W) PA6+GF30%, High Impact
Feature: Injection Molding, PA6+GF30%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
|
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester
Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan..
|
|||
| Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
|
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced
Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne..
|
|||
| Nozzle Temperature | 280 - 290 °C | 536 - 554 °F | |
|
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Nozzle Temperature | 280 - 290 °C | 536 - 554 °F | |
|
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
|
|||
| Nozzle Temperature | 280 - 290 °C | 536 - 554 °F | |
|
Tisan TISARBON® Flame Retardant (V0) Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
|
|||
| Nozzle Temperature | 280 - 290 °C | 536 - 554 °F | |
|
Tisan TISARBON® UNR Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
|
|||
| Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
|
|||
| Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Arkema Group Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7233 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Arkema Group Pebax® 7233 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7233 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
|
|||
| Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
|
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
|
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
|
|||
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Average value: 275 °C Grade Count:11 |
|
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Nozzle Temperature | 180 - 290 °C | 356 - 554 °F | Average value: 238 °C Grade Count:34 |
|
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
|
|||
| Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | |
|
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||