| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 326 °C Grade Count:22 |
|
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 330 °C Grade Count:28 |
|
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
|
|||
| Nozzle Temperature | 270 - 340 °C | 518 - 644 °F | Average value: 290 °C Grade Count:17 |
|
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7399 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 21-7979 Polyamide 6/6T, with glass fiber, 8-mm-granulate
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.High dimensionally stable prec..
|
|||
| Nozzle Temperature | 330 - 340 °C | 626 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 21-8115 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Nozzle Temperature | 325 - 340 °C | 617 - 644 °F | NH Cylinder Temp for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | |
|
Lehmann & Voss LUVOCOM® 1301-8212/BL PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
|
|||
| Nozzle Temperature | 320 - 340 °C | 608 - 644 °F | Average value: 330 °C Grade Count:3 |
|
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
|
|||