| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow
Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
|
|||
| Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
|
Polymer Resources PCSF-FRG30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade
Polycarbonate, 30% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con..
|
|||
| Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
|
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced
Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
|
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
|
|||
| Mold Temperature | 71.1 - 104 °C | 160 - 220 °F | |
|
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
|
|||
| Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
|
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy
Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio..
|
|||
| Mold Temperature | 71.1 - 87.8 °C | 160 - 190 °F | |
|
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Ravago Manufacturing Americas Hylon® N2033HL Nylon 6 (Cond)
Information provided by Ravago.
|
|||
| Mold Temperature | 71.1 - 98.9 °C | 160 - 210 °F | |
|
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
|
|||
| Mold Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
|
LTL Color Compounds ColorFast® FRA202 General Purpose ABS
General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc.
|
|||
| Mold Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
|
LTL Color Compounds ColorFast® FRA204 ABS
High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc.
|
|||
| Mold Temperature | 71.0 - 94.0 °C | 160 - 201 °F | |
|
Styron Pulse® B-270 PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Mold Temperature | 71.1 - 93.3 °C | 160 - 200 °F | |
|
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||