| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 10 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 10 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 10 K/40 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LATILUB 88/50-20GRT K/10 PEEK Based, 10% Carbon Fiber Reinforced, 20% Graphite and PTFE Self Lubricating Plastic
Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LATILUB 88/50-30GRT PEEK Based, 30% Graphite and PTFE Self Lubricating Plastic
(Unverified Data**)&l
Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low..
|
|||
| Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
|
|||
| Mold Temperature | 180 °C | 356 °F | |
|
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
|
|||
| Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
|
|||
| Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
|
|||
| Mold Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
|
|||
| Mold Temperature | 180 - 210 °C | 356 - 410 °F | normal |
|
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
|
|||
| Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
(Unverified Data**)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491°F), E..
|
|||
| Mold Temperature | >= 180 °C | >= 356 °F | |
|
Solvay Specialty Polymers Supradel® HTS-2630 High Temperature Sulfone Resin
(discontinued **)
SUPRADEL HTS-2630 is a 30% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer.In addition to exceptional thermal performance, this resin has the other performance ..
|
|||
| Mold Temperature | >= 180 °C | >= 356 °F | |
|
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
|
|||
| Mold Temperature | >= 180 °C | >= 356 °F | |
|
Solvay Specialty Polymers Supradel® HTS-2430 High Temperature Sulfone Resin
(discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of ..
|
|||
| Mold Temperature | >= 180 °C | >= 356 °F | |
|
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **)
SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t..
|
|||
| Mold Temperature | >= 180 °C | >= 356 °F | |
|
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
|
|||
| Mold Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Lehmann & Voss LUVOCOM® TPI-8257 Thermoplastic polyimide, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.High-strength and high-stiff parts; lo..
|
|||
| Mold Temperature | 180 - 230 °C | 356 - 446 °F | |
|
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Mold Temperature | 180 - 230 °C | 356 - 446 °F | |
|
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
|
|||
| Mold Temperature | 180 - 230 °C | 356 - 446 °F | |
|
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced
High thermal conductivity product based on Polyetheretherketone (PEEK). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||
| Mold Temperature | 180 - 210 °C | 356 - 410 °F | |
|
Solvay Specialty Polymers EpiSpire® EP-340 Sulfone, High Temperature (HTS)
EpiSpire® EP-340 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 265°C (509°F) and a heat deflection temperature of 255°C (491..
|
|||
| Mold Temperature | 180 - 190 °C | 356 - 374 °F | |
|
LATI LARPEEK 50 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Mold Temperature | 180 °C | 356 °F | |
|
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..
|
|||
| Mold Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..
|
|||