| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
|
PolyOne Gravi-Tech™ GRV-NJ-110-W Polyamide 12 (Nylon 12)
Information provided by PolyOne
|
|||
| Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
|
PolyOne Gravi-Tech™ GRV-NY-085-W-NAT Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Mold Temperature | 82.2 - 107 °C | 180 - 225 °F | |
|
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 82.2 - 121 °C | 180 - 250 °F | |
|
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE
Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow
Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
|
|||
| Mold Temperature | 82.2 - 121 °C | 180 - 250 °F | Average value: 103 °C Grade Count:3 |
|
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m..
|
|||
| Mold Temperature | 82.0 - 104 °C | 180 - 219 °F | |
|
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer
Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go..
|
|||
| Mold Temperature | 82.2 - 107 °C | 180 - 225 °F | |
|
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||