| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
|
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66
Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char..
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
|
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
|
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66
Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a..
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
|
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | Injection Molding; ISO 10724 |
|
Lanxess Pocan® T 7391 POS151 000000 PBT + PET, 45% Glass Fiber
(discontinued **)
PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | optimum; Injection Molding |
|
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**)
Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | optimum; Injection Molding |
|
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | optimum; Injection Molding |
|
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**)
Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | optimum; Injection Molding |
|
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal
(Unverified Data**)
Delrin® FG400XRD NC010 is a filled, medium viscosity acetal copolymer for injection molding. It is detected in x-ray detectors. It has been developed for consideration into applications such as par..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 1-RG 1 Polyamide 66, with PAN-carbon fiber, RG-standard
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | Start Point: 100°C |
|
Kingfa JH720 G15 15% Glass Fiber Reinforced PC
Features:Excellent balance propertiesHigh mechanical propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug partsIn..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | Injection Molding |
|
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Mechanical and Structural Standard Molding |
|
Mitsui Arlenâ„¢ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | for test specimens; ISO 294 |
|
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber
PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS.
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 1/CF/10/GK/20/TF/5/BK Polyamide 66, with carbon fiber, glass spheres and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS-B Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 1-1119 VP Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Lehmann & Voss LUVOCOM® 1-7139-1 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
|
|||
| Mold Temperature | 90.0 - 140 °C | 194 - 284 °F | for Electronic and Electric Standard Molding |
|
Mitsui Arlenâ„¢ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
|
|||
| Mold Temperature | 90.0 °C | 194 °F | Ejection temperature |
|
Styrolution Terlux® 2812 TR MABS
Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
|
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
|
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
|
|||
| Mold Temperature | 90.0 - 120 °C | 194 - 248 °F | |
|
Eurotec® Tecopet® PT70 GR30 NL100 MB PET, 30% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Mold Temperature | 90.0 °C | 194 °F | Optimal |
|
BASF Ultraform® Z2320 003 POM
Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF
|
|||
| Mold Temperature | 90.0 °C | 194 °F | Optimal |
|
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned)
Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con..
|
|||
| Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
|
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET
Information provided by A. Schulman.
|
|||