| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | DAM; optimum |
|
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
|
|||
| Mold Temperature | >= 95.0 °C | >= 203 °F | |
|
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**)
Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a..
|
|||
| Mold Temperature | >= 95.0 °C | >= 203 °F | |
|
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**)
Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers
|
|||
| Mold Temperature | >= 95.0 °C | >= 203 °F | |
|
DuPont Performance Polymers Rynite® RE5231 BK533 PET
(Unverified Data**)
Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l..
|
|||
| Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
|
Lavergne VYPET VNT 645 PET 45% Glass Reinforced
Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E..
|
|||
| Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
|
Lavergne VYPET VNT 615 PET 15% Glass Reinforced
Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio..
|
|||
| Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
|
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent..
|
|||
| Mold Temperature | 95.0 - 125 °C | 203 - 257 °F | |
|
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che..
|
|||
| Mold Temperature | 95.0 - 140 °C | 203 - 284 °F | |
|
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | Injection molding |
|
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | Injection molding |
|
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | Injection molding |
|
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and ..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | Injection molding |
|
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st..
|
|||
| Mold Temperature | 95.0 - 140 °C | 203 - 284 °F | |
|
Akro-Plastic Akromid® T6 GF 40 (3500) PPA Dry, 40% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined ..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined ..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance ..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
|
BASF Capron® GR30 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc..
|
|||
| Mold Temperature | 95.0 - 110 °C | 203 - 230 °F | |
|
LATI Latigea B02 H6 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
|
|||
| Mold Temperature | >= 95.0 °C | >= 203 °F | |
|
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**)
Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont..
|
|||
| Mold Temperature | 95.0 °C | 203 °F | |
|
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber
A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
|
|||