Polymer Property : Mold Temperature = 225 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 60.0 - 107 °C
140 - 225 °F
PolyOne Nymax™ 1200 A HS Black 13 A Polyamide 66 (Nylon 66)
The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi..
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Oxford Polymers C-Acetal 25GF-BK Acetal, 25% Glass Fiber Reinforced
Product Description: Glass Fiber (25% Reinforced), Acetal Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristics: Pre-color..
Mold Temperature 65.6 - 107 °C
150 - 225 °F
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated  (discontinued
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Mold Temperature 65.6 - 107 °C
150 - 225 °F
Average value: 89.4 °C Grade Count:10
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened
Data provided by Clariant Masterbatches
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Clariant Renol 6608G43 Nylon 66, 43% Glass Fiber, Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches