| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 15.6 - 26.7 °C | 60.0 - 80.0 °F | |
|
RheTech Products E204-01 High Density Polyethylene, Black
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.0 - 80.0 °F | |
|
RheTech Products E206-01 Linear Low Density Polyethylene, Black
Applications: Flexible componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 ..
|
|||
| Mold Temperature | 21.1 - 26.7 °C | 70.0 - 80.1 °F | |
|
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established...
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G2712-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2712-1000-02 is an easy processing TPE designed for injection molding and extrusion aplications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - High..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - ..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G7930-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7930-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G2701C Thermoplastic Elastomer (TPE)
Dynaflex™ G2701C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Rubbery Feel..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE)
Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A..
|
|||
| Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
|
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE)
Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta..
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703TU95 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po..
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703ZB92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU) Base ResinFlexibleInformation provided by Technical Polymers
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703ZC76 Stainless Steel Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703ZC87 Stainless Steel Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703ZD88 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym..
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703ZD90 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polym..
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4703ZG92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
|
|||
| Mold Temperature | 10.0 - 26.7 °C | 50.0 - 80.0 °F | |
|
Ecomass® 4710BI71 Filled Polyurethane, Injection Molding
Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead for weighting, balancing and vibration..
|
|||