| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Average value: 80.4 °C Grade Count:14 |
|
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® 6134 NC010 PBT
(Unverified Data**)
Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**)
Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**)
Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**)
Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**)
Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® SK601 BK851 PBT
(Unverified Data**)
Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® SK605 BK851 PBT
(Unverified Data**)
Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | Injection Molding |
|
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**)
Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® SK642FR BK851 PBT
(Unverified Data**)
Crastin® SK642FR BK851 is a black 15% glass fiber reinforced, flame retardant polybutylene terephthalate for injection molding. It has a UL94 V-0 rating @ 0.75mm.Information provided by DuPont Perf..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**)
Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Mold Temperature | 90.0 - 130 °C | 194 - 266 °F | |
|
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **)
PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 90°C |
|
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
|
|||
| Mold Temperature | 110 - 130 °C | 230 - 266 °F | |
|
LATI Lasulf PSU
Polysulfone (PSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | Start Point: 100°C |
|
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
|
|||
| Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
|
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral
PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS.
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in..
|
|||
| Mold Temperature | 95.0 - 130 °C | 203 - 266 °F | |
|
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable ..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled
MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled
ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe..
|
|||
| Mold Temperature | 80.0 - 130 °C | 176 - 266 °F | |
|
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva..
|
|||
| Mold Temperature | 30.0 - 130 °C | 86.0 - 266 °F | |
|
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
|
|||
| Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
|
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Mold Temperature | 100 - 130 °C | 212 - 266 °F | |
|
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
|
|||
| Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
|
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
|
|||
| Mold Temperature | 85.0 - 130 °C | 185 - 266 °F | DAM |
|
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
|
|||