Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 30.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Plastcom PLASTALEN® EH 91 N Polyethylene
HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o.
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Plastcom PLASTALEN® PH 91 SD Polypropylene
Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o.
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant
FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
PolyOne OnFlex™ U 5380A-S0013 Thermoplastic Elastomer (TPE)
OnFlex™-U thermoplastic elastomer compounds are based on thermoplastic polyurethane elastomers (TPE-U). The OnFlex™-U 5300 series are based upon alloys of SEBS and TPU, combining the advantages of..
Mold Temperature 30.0 - 70.0 °C
86.0 - 158 °F
Premix Thermoplastics PRE-ELEC® ESD 7100
PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization
FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica..
Mold Temperature 30.0 - 130 °C
86.0 - 266 °F
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT  (Unverified Data**)
Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo..
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Start Point: 50°C
Kingfa HR-527A Modified ABS
Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Mold Temperature 30.0 - 80.0 °C
86.0 - 176 °F
Start Point: 50°C
Kingfa HR-527B Modified ABS
Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Start Point: 50°C
Kingfa FRHIPSV-0 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis Daplen™ EE115T TPO Compound
Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis Daplen™ EG203AE Polypropylene Compound Elastomer and Mineral Modified
Daplen EG203AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EG203AE is a material with excellent impact /stiffness ratio. Thanks to its low ..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled
Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced
GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. ..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding
LDPE 1070 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade adapted to the production of flexible parts with a high production rate.Applicat..
Mold Temperature 30.0 - 65.6 °C
86.0 - 150 °F
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT
Information provided by A. Schulman.
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis Daplen™ EE109AE TPO Compound
Daplen EE109AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE109AE is a material with excellent impact /stiffness ratio. Thanks to its low ..
Mold Temperature 30.0 - 130 °C
86.0 - 266 °F
DuPont Performance Polymers Crastin® CE2056 NC010 PBT
Crastin® CE2056 NC010 is an unreinforced polybutylene terephthalate molding resin.Information provided by DuPont Performance Polymers
Mold Temperature 30.0 - 130 °C
86.0 - 266 °F
Injection Molding
DuPont Performance Polymers Crastin® SK612SF BK591 PBT
Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast ..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding
Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar.
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Eurostar Starpylen MCR13S PP, 15% Carbon Fiber Filled, Injection Molded
Starpylen MCR13S is a 15% Carbon Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded
Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar.
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding
Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Mold Temperature 30.0 - 90.0 °C
86.0 - 194 °F
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
Mold Temperature 30.0 - 130 °C
86.0 - 266 °F
DuPont Performance Polymers Crastin® LW9030 BK851 PBT  (Unverified Data**)
Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Mold Temperature 30.0 - 150 °C
86.0 - 302 °F
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSX65T20 is a 20% mineral filled grade intended for injection molding. Daplen KSX65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSX65T20 offe..
Copyright © lookpolymers.com All Rights Reserved