| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 49.0 - 93.0 °C | 120 - 199 °F | |
|
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 93.0 °C | 120 - 199 °F | |
|
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 93.0 °C | 120 - 199 °F | |
|
PolyOne Lubri-Tech™ PS-000/20T Polyester (PBT) - 20% PTFE Lubricated
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 71.0 °C | 120 - 160 °F | |
|
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 66.0 °C | 120 - 151 °F | |
|
PolyOne Lubri-Tech™ AS-000/10T-2S ABS - 10% PTFE - 2% Silicone
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
|
PolyOne Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
|
PolyOne Lubri-Tech™ ATH-000/20T Homopolymer Acetal - 20% PTFE Lubricated
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 121 °C | 120 - 250 °F | Average value: 85.7 °C Grade Count:24 |
|
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
|
|||
| Mold Temperature | 49.0 - 107 °C | 120 - 225 °F | Average value: 77.5 °C Grade Count:14 |
|
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
|
|||
| Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
|
PolyOne Lubri-Tech™ NL-000/15T Nylon 612 - 15% PTFE Lubricated
(discontinued **)
Properties Dry as MoldedData provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.
|
|||
| Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
|
PolyOne Lubri-Tech™ NL-40GB/15T Nylon 6/12 - 40% Glass Bead Reinforced - 15% PTFE Lubricated
(discontinued **
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 121 °C | 120 - 250 °F | Average value: 90.2 °C Grade Count:66 |
|
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
|
|||
| Mold Temperature | 49.0 - 120 °C | 120 - 248 °F | Average value: 86.3 °C Grade Count:15 |
|
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
|
|||
| Mold Temperature | 49.0 - 107 °C | 120 - 225 °F | Average value: 89.5 °C Grade Count:14 |
|
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| Mold Temperature | 49.0 - 82.0 °C | 120 - 180 °F | |
|
PolyOne Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
(discontinued **)
Data provided by PolyOne.
|
|||
| Mold Temperature | 49.0 - 120 °C | 120 - 248 °F | Average value: 88.1 °C Grade Count:29 |
|
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
|
|||