Polymer Property : Mold Temperature = 70.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Plastcom SLOVAMID 6 GF 15 T 25 LTS PA6, 15% glass fibre, 25% mineral filling
FeaturesGood anisotropy of the manufacturing shrinkage. The talc is added to get the material shrinkage identical in both directions. Application for flat products in disc form /no screw after cooli..
Mold Temperature 70.0 - 80.0 °C
158 - 176 °F
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
Mold Temperature 70.0 °C
158 °F
Moulding a 6 gram (shot weight) gasket with a 50 ton injection moulding machine having a screw diameter of 25[mm]
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
LATI LATILUB 73/13-10ST Polyoxymethylene Base (POM), 10% Mixed PTFE/Silicone Self Lubricating Plastic  (Un
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic  (discon
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6  (Unverified Data**)
Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Start Point: 80°C
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to..
Mold Temperature 70.0 - 80.0 °C
158 - 176 °F
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding
General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance..
Mold Temperature 70.0 - 80.0 °C
158 - 176 °F
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Injection Molding
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Lehmann & Voss Nylatron® MR 2007 Polyamide 6, with mineral filler
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Mold Temperature 70.0 - 100 °C
158 - 212 °F
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Mold Temperature 70.0 - 100 °C
158 - 212 °F
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE
SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Sax Polymers SAXAMID 126K6 Nylon 6, 30% Glass Filled
SAXAMID 126K6 is a 30% glass beads filled polyamide 6 injection-molding-grade. It is characterized by dimensional stability, low warpage and good surface quality.Information provided by SAX Polymers..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber
SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber
SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber
SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig..
Mold Temperature 70.0 - 80.0 °C
158 - 176 °F
Styron PULSEâ„¢ GX50 PC/ABS Engineering Resin
Overview: PULSE GX50 engineering resins give exceptional impact strength even at low temperature and have sufficient heat resistance for the majority of automotive interior components. This resin pr..
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Solvay TECHNYL® 2710IR PA66, DRY
Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use..
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
actual surface temp
Unitika FUN-8000
Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd.
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech..
Mold Temperature 70.0 - 100 °C
158 - 212 °F
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Mold Temperature 70.0 - 100 °C
158 - 212 °F
CP-Polymer-Technik Wellamid® 6600 GS 40 HWCP 40% Glass Sphere Filled Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding
Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Mold Temperature 70.0 °C
158 °F
See Materials Notes
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)  (discontinued **)
Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also ..