| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
|
PolyOne Gravi-Tech™ GRV-NJ-110-W Polyamide 12 (Nylon 12)
Information provided by PolyOne
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Mold Temperature | 82.2 °C | 180 °F | |
|
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow
Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po..
|
|||
| Mold Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
|
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
|
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
|
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(discontinu
Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; ..
|
|||