| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane
Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi..
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical AF312 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HG193S ABS, High Flow, Chemical Resistance
Feature: Injection Molding, High Flow, Chemical ResistanceApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HI100 ABS, High Impact
Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HI121U ABS
Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 403AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 460AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1045D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX TO1065A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX TO1192A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical MA210 ABS, Low Gloss
Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC
Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HF350U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LI912 ASA
Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane