| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 199 - 260 °C | 390 - 500 °F | |
|
Multibase Multi-Pro® 2005 RCI Polypropylene
Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided ..
|
|||
| Rear Barrel Temperature | 199 - 260 °C | 390 - 500 °F | |
|
Multibase Multi-Pro® 3012 RC Polypropylene
Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber
Natural color. E6126 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati..
|
|||
| Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
|
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
|
Multibase Multi-Pro® 4005 MI Polypropylene
Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
|
|||
| Rear Barrel Temperature | 232 - 260 °C | 450 - 500 °F | |
|
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Rear Barrel Temperature | 249 - 260 °C | 480 - 500 °F | |
|
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef..
|
|||
| Rear Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Injection Molding |
|
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant
Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Injection Molding |
|
LG Chemical LUMID HI1102A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
|
LG Chemical Lupox® TE5000HU PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 26062-94-2, 137050-02-03 and 103598-77-2Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
|
LG Chemical Lupox® TE5000SP PBT+PC
Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
|
LG Chemical Lupox® TE5000SZ PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
|
LG Chemical Lupox® TE5011M PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG ..
|
|||
| Rear Barrel Temperature | 190 - 260 °C | 374 - 500 °F | Injection |
|
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend
INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form...
|
|||
| Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
|
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 243 - 260 °C | 470 - 500 °F | |
|
Mitsubishi Iupilon® H3000UR 30 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
|
LG Chemical Lupox® TE5011 PBT+PC
Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro..
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go..
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned)
Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
|
|||
| Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
|
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
|
Diamond Polymers ASA TW-17
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
|
Diamond Polymers ASA TW-20
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
|
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer
Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go..
|
|||
| Rear Barrel Temperature | 229 - 260 °C | 445 - 500 °F | |
|
Diamond Polymers ABS/PC 9801
Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Rear Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
|
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **)
Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope..
|
|||