| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
|
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66)
The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah..
|
|||
| Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
|
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 260°C |
|
Kingfa JH820 Modified PC
Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 260°C |
|
Kingfa JH830T Flame Retardant PC
Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor..
|
|||
| Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
|
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG ..
|
|||
| Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | Injection Molding |
|
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity
Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
|
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
|
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose
Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
|
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose
Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
|
LG Chemical LUMID HI2302A(W) PA6+GF30%, High Impact
Feature: Injection Molding, PA6+GF30%, High ImpactApplication: Automotive PartsCAS No. 25038-54-4, 9010-79-1 and 65997-17-3Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 230 - 270 °C | 446 - 518 °F | |
|
LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
|
LG Chemical LUPOY GP5006B PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
|
LG Chemical LUPOY GP5006BH PC/ABS, Heat Resistance, Impact Strength
Description: Injection Molding, PC/ABS, Heat Resistance, Impact Strength, High ToughnessApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
|
|||
| Rear Barrel Temperature | 230 - 270 °C | 446 - 518 °F | |
|
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
|
LG Chemical LUPOY HG5000B PC/ABS, Heat Resistance
Description: Injection Molding, PC/ABS, High Gloss, Heat Resistance, High FlowApplication: E&E (housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Rear Barrel Temperature | 230 - 270 °C | 446 - 518 °F | Injection Molding |
|
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 255°C |
|
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
|
|||
| Rear Barrel Temperature | 255 - 270 °C | 491 - 518 °F | |
|
LG Chemical LUPOY GN-2006F Halogen Free Modified PC, Unreinforced, Weather Resistant, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
|
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
|
|||
| Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
|
|||
| Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
|
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
|
|||
| Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
|
Unitika U-8000
U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than..
|
|||
| Rear Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
|
LG Chemical LUPOY NS5000C PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||