| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Rear Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
|
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE
Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
|
|||
| Rear Barrel Temperature | 260 - 299 °C | 500 - 570 °F | |
|
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy
Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FR7 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 260F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP4 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FRG20 Modified PPO, UL 94 V-1, 20% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP1 Modified PPO, General Purpose with HDT of 265 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 288 - 299 °C | 550 - 570 °F | |
|
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LGF30 - PA66 Nylon 66, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Rear Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
|
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Rear Barrel Temperature | 260 - 299 °C | 500 - 570 °F | |
|
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FR7 Modified PPO, V-0 Flame Retardant, Medium Heat, 250 HDT
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-MF-FR3 Modified PPO, UL 94 V-0 with HDT of 230 F, Mineral Reinforced
(Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 249 - 299 °C | 480 - 570 °F | |
|
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||