| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 302 - 316 °C | 575 - 600 °F | |
|
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristics: High Str..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced
Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release
Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified
Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced
Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced
Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release
Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced
Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced
Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release
Polycarbonate, 40% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-G30-[color]-1 Polycarbonate, 30% Glass Reinforced with Mold Release
Polycarbonate, 30% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant
Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled
20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc.
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled
30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc.
|
|||
| Rear Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC731 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC733R Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PCGF10 Molding Grade PC with 10% Glass
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PCGF20 Molding Grade PC with 20% Glass
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PCGF30 Molding Grade PC with 30% Glass
Information provided by Star Plastics, Inc.
|
|||
| Rear Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PCSF-FRG20 Polycarbonate, 20% Glass Reinforced Structural Foam Grade
Polycarbonate, 20% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con..
|
|||