| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
|
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
|
|||
| Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
|
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Rear Barrel Temperature | 171 - 182 °C | 340 - 360 °F | |
|
LTL Color Compounds ColorFast® FRA205 ABS
Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® OBC 4565A Thermoplastic Elastomer
Uses: Flexible Grips; Overmolding Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion; Extrusion; Injection Molding Injection ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-1081B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-1120E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-1268A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-1295B Thermoplastic Elastomer
Uses: Consumer Applications; General Purpose; Soft Touch Applications; Flexible Grips; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: M..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2452L Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2460B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2560F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2565A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2590A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2596C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2597 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-2717B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Inject..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-3260-1 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-3954-55 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-4145 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-6085 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-81-D965-P Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer
Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-88-N882-A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Rear Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
|
Teknor Apex Telcar® TL-1996F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||