| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
|
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by ..
|
|||
| Rear Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
|
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide..
|
|||
| Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
|
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
|
|||
| Rear Barrel Temperature | 180 - 210 °C | 356 - 410 °F | Injection Molding |
|
LG Chemical XR401T ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9..
|
|||
| Rear Barrel Temperature | 180 - 190 °C | 356 - 374 °F | Extrusion |
|
Stellarchem LP-830 TPE Compound
This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
|
|||
| Rear Barrel Temperature | 180 °C | 356 °F | Extrusion Coating |
|
DuPont Appeel® LSR20D752 Lidding Sealant Resin
Appeel® LSR20D752 is a modified ethylene acrylate copolymer designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
|
|||
| Rear Barrel Temperature | 180 - 190 °C | 356 - 374 °F | |
|
Chi Mei Acryrex® CM-211 PMMA
Features:Good Weather ResistanceHigh ClarityHigh FlowHigh GlossHigh Heat ResistanceHigh ViscosityUses:ContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: Pellets..
|
|||
| Rear Barrel Temperature | 180 °C | 356 °F | Injection |
|
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Rear Barrel Temperature | 180 °C | 356 °F | Injection |
|
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Rear Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical KEYFLEX TO1075AR Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical
|
|||