Polymer Property : Rear Barrel Temperature = 450 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy
Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In..
Rear Barrel Temperature 232 - 260 °C
450 - 500 °F
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow
Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani..
Rear Barrel Temperature 232 - 260 °C
450 - 500 °F
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow
Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:..
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 232 - 266 °C
450 - 510 °F
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized
Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Rear Barrel Temperature 232 - 266 °C
450 - 510 °F
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade
ALATHON H4250 is a high-flow “freezer” grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade
ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® M5372 High Density Polyethylene
ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. ..
Rear Barrel Temperature 232 °C
450 °F
LyondellBasell Alathon® M6138 High Density Polyethylene
ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness...
Rear Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
LTL Color Compounds ColorFast® PBT100 PBT
General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Rear Barrel Temperature 232 - 260 °C
450 - 500 °F
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 232 - 274 °C
450 - 525 °F
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Rear Barrel Temperature 232 - 243 °C
450 - 470 °F
Entec Hylox® 9230BK PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Rear Barrel Temperature 232 - 260 °C
450 - 500 °F
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow  (Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Rear Barrel Temperature 232 - 249 °C
450 - 480 °F
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc.