Processing Properties Metric English Comments
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled
PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced
Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow
Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance  (Unverified Data**)&
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Oxford Polymers PC C20-000 Clear PC
Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl..
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG20 Modified PPO, UL 94 V-1, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
Polymer Resources PC/ABS-G30 General Purpose PC/ABS Alloy, 30% Glass Filled
PC/ABS Alloy, General Purpose, 30% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release
Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 288 °C
480 - 550 °F
LTL Color Compounds ColorFast® PAHF Polycarbonate-ABS Alloy
General purpose HB-rated PC/ABS with improved chemical resistanceAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 249 - 271 °C
480 - 520 °F
Samyang Trirex® PC-3022U 15 MFI UV Stabilized Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 249 - 266 °C
480 - 510 °F
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-MF-FR3 Modified PPO, UL 94 V-0 with HDT of 230 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 249 - 299 °C
480 - 570 °F
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved