Polymer Property : Rear Barrel Temperature = 520 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced
Nylon 66, 25% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled
Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized
Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-G43-[color]H Nylon, 43% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened
Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow
Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled
Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone
Rear Barrel Temperature 271 - 288 °C
520 - 550 °F
Star Plastics PC1212FR Molding Grade PC FR
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 271 - 288 °C
520 - 550 °F
Star Plastics PC1212FRR Molding Grade PC FR
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 271 - 288 °C
520 - 550 °F
Star Plastics PC1510R Molding Grade PC
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 271 - 288 °C
520 - 550 °F
Star Plastics PC1510UV Molding Grade PC
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 271 - 288 °C
520 - 550 °F
Star Plastics PC1212R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated
Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Wellman Wellamid® FRGF25-66-N Flame Retardant Nylon 66, Lubricated, 25% Glass Fiber
Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Rear Barrel Temperature 271 - 282 °C
520 - 540 °F
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
LTL Color Compounds ColorFast® FRPC300 Polycarbonate, Flame-Retarded
V2-rated polycarbonateAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 271 - 293 °C
520 - 560 °F
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded
Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.