| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 121 °C | 250 °F | |
|
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **)
ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th..
|
|||
| Drying Temperature | 121 °C | 250 °F | |
|
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Drying Temperature | 121 °C | 250 °F | |
|
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
|
LNP Lubricomp® EFL-4544 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Drying Temperature | 121 °C | 250 °F | |
|
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **)
Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Drying Temperature |
121
°C @Time 14400 sec |
250
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
|
|||
| Drying Temperature | 121 °C | 250 °F | |
|
Styron EMERGEâ„¢ 4850-19 Polycarbonate
EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr..
|
|||
| Drying Temperature | 121 °C | 250 °F | |
|
Styron EMERGEâ„¢ 4510-10 Polycarbonate
EMERGEâ„¢ PC 4510-10 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform..
|
|||
| Drying Temperature | 121 - 149 °C | 250 - 300 °F | |
|
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
|
|||