| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced
Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced
Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant
Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-GFMF2 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced
Polybutylene Terephthalate, 40% Glass/Mineral ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified
Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
|
|||
| Drying Temperature | 82.2 - 121 °C | 180 - 250 °F | |
|
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Drying Temperature | 104 - 121 °C | 219 - 250 °F | Average value: 113 °C Grade Count:7 |
|
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
|
|||
| Drying Temperature | 93.3 - 121 °C | 200 - 250 °F | Average value: 104 °C Grade Count:7 |
|
Overview of materials for Polyphenylene Ether, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values ..
|
|||
| Drying Temperature | 80.0 - 121 °C | 176 - 250 °F | Average value: 107 °C Grade Count:14 |
|
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
|
|||
| Drying Temperature | 82.2 - 121 °C | 180 - 250 °F | Average value: 116 °C Grade Count:7 |
|
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Drying Temperature | 75.0 - 121 °C | 167 - 250 °F | Average value: 104 °C Grade Count:50 |
|
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
|
|||
| Drying Temperature | 116 - 121 °C | 241 - 250 °F | Average value: 121 °C Grade Count:19 |
|
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
|
|||
| Drying Temperature | 121 - 121 °C | 250 - 250 °F | Average value: 121 °C Grade Count:9 |
|
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Drying Temperature | 70.0 - 121 °C | 158 - 250 °F | Average value: 88.5 °C Grade Count:15 |
|
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
|
|||
| Drying Temperature | 116 - 121 °C | 240 - 250 °F | |
|
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity
Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc.
|
|||
| Drying Temperature | 71.0 - 121 °C | 160 - 250 °F | Average value: 97.7 °C Grade Count:14 |
|
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
|
|||
| Drying Temperature | 80.0 - 121 °C | 176 - 250 °F | Average value: 108 °C Grade Count:27 |
|
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
|
|||
| Drying Temperature | 70.0 - 121 °C | 158 - 250 °F | Average value: 97.0 °C Grade Count:19 |
|
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
|
|||
| Drying Temperature | 80.0 - 121 °C | 176 - 250 °F | Average value: 115 °C Grade Count:6 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..
|
|||