| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PP CQX10030 RT Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC TS4030 H Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC T10030 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH K8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH MGF5040 Polypropylene Homopolymer, Multifiller
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Average value: 79.8 °C Grade Count:5 |
|
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
|
|||
| Drying Temperature |
70.0
°C @Time 7200 sec |
158
°F @Time 2.00 hour |
Pre-dry |
|
Kingfa FRHIPS-220 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Injection Molding |
|
LG Chemical LUMID HI5001AS PA6/PO, High Barrier Property, CaCl2 Resistance, High Impact
Feature: Injection Molding, PA6/PO, High Barrier Property, CaCl2 Resistance, High ImpactApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1, 9002-88-4 and 105-60-2Information pro..
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | Injection Molding |
|
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability
Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided ..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
|
LG Chemical LUPOL GP3202 PP+MF20%
Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
|
LG Chemical LUPOL GP3302 PP+MF30%
Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
|
|||
| Drying Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
|
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
|
LG Chemical LUPOL HI5204G PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
|
|||
| Drying Temperature | 70.0 - 100 °C | 158 - 212 °F | |
|
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Drying Temperature | 70.0 - 100 °C | 158 - 212 °F | |
|
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Extrusion Molding |
|
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Lubrizol Estane® S198A Thermoplastic Polyurethane
Type: Estane® S198A is a Shore 98A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
|
|||
| Drying Temperature | 70.0 °C | 158 °F | |
|
Eastman DuraStar MN620 Polymer, Natural
Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly..
|
|||
| Drying Temperature |
70.0
°C @Time 10800 sec |
158
°F @Time 3.00 hour |
|
|
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding
Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature |
70.0
°C @Time 10800 sec |
158
°F @Time 3.00 hour |
|
|
Eurostar Starpylen HZ 30WF2 PP, 30% Wood Fiber Filled, Injection Molding
Starpylen HZ 30WF2 is a 30% Wood Fiber Reinforced Polypropylene Injection Molding Resin (also known as HZ30WF2)Information provided by Eurostar.
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC GF5020 PB Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 130 °C | 158 - 266 °F | Average value: 120 °C Grade Count:60 |
|
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
|
|||
| Drying Temperature | <= 70.0 °C | <= 158 °F | |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..
|
|||
| Drying Temperature |
70.0
-
80.0
°C @Time 10800 sec |
158
-
176
°F @Time 3.00 hour |
|
|
LATI Latistat 48/9900-03 EVA
Dissipative product based on Ethyl-Vinyl-Acetate (EVA). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
|
|||