| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Pre-drying in a dehumidifier |
|
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Pre-drying in a dehumidifier |
|
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b..
|
|||
| Drying Temperature |
70.0
-
80.0
°C @Time 10800 - 14400 sec |
158
-
176
°F @Time 3.00 - 4.00 hour |
Pre-drying in a dehumidifier |
|
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
|
|||
| Drying Temperature |
60.0
-
80.0
°C @Time 10800 - 14400 sec |
140
-
176
°F @Time 3.00 - 4.00 hour |
Pre-drying; If stored for longer than 1 year |
|
Premix Thermoplastics PRE-ELEC® PS 1328
PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC K2040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH GF3045 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH GF5015 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH K20020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPH K8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature |
70.0
-
80.0
°C @Time 7200 - 14400 sec |
158
-
176
°F @Time 2.00 - 4.00 hour |
Pre-dry |
|
Kingfa FW-620 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
|
LG Chemical LUPOL GP2100 PP+GF10%
Description: Injection Molding, PP+GF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Extrusion Molding |
|
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Extrusion Molding |
|
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Extrusion Molding |
|
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Drying Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
|
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Drying Temperature |
70.0
-
80.0
°C @Time 10800 sec |
158
-
176
°F @Time 3.00 hour |
|
|
LATI Lastilac AR-V0E ABS, Flame Retardant
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Lubrizol Estane® S364D Thermoplastic Polyurethane
Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
|
|||
| Drying Temperature | 79.4 - 80.0 °C | 175 - 176 °F | Average value: 79.8 °C Grade Count:3 |
|
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPC T5020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
|
Polykemi AB POLYfill PPHC K8040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
|
|||