| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 150 °C | 302 °F | |
|
PolyOne OnForce™ LFT SF-40LGF/001 Natural Polyphenylene Sulfide (PPS)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
|
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
|
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Drying Temperature | 150 °C | 302 °F | |
|
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard..
|
|||
| Drying Temperature | 150 °C | 302 °F | |
|
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro..
|
|||
| Drying Temperature | 150 °C | 302 °F | |
|
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
|
|||
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® Vicote® 708 Polyetheretherketone (PEEK) Powder
VICOTE 708 and 709 grades are specially developed powder coatings (based on VICTREX HT™ polymer) with a higher Tg and melting point than the standard VICOTE products. VICOTE 708 and 709 grades deli..
|
|||
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® Vicote® F814 Polyetheretherketone (PEEK) Liquid Dispersion
VICOTE F814 has been specifically formulated to provide a resilient coating with high wear and abrasion resistance on ferrous and non-ferrous metals such as carbon and cast steel. These properties a..
|
|||
| Drying Temperature |
150
°C @Time 10800 - 18000 sec |
302
°F @Time 3.00 - 5.00 hour |
Dehumidifying dryer |
|
Lehmann & Voss LUVOCOM® 1100-7725 VP Polyether sulfone, with glass fiber, lubricant modified
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Drying Temperature |
150
-
180
°C @Time 10800 sec |
302
-
356
°F @Time 3.00 hour |
|
|
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK)
KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades ..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-820 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-820 GF15 is a low flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpir..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
KetaSpire® KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry ..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
|
|||
| Drying Temperature |
150
°C @Time 14400 sec |
302
°F @Time 4.00 hour |
|
|
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
|
|||
| Drying Temperature | 150 - 160 °C | 302 - 320 °F | |
|
Eastman Eastar EN052 Polyester
Eastar Polyester EN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
|
|||
| Drying Temperature |
150
°C @Time 10800 sec |
302
°F @Time 3.00 hour |
|
|
Victrex® Vicote® F813 Black Polyetheretherketone (PEEK) Liquid Dispersion
VICOTE® is the brand name for the Victrex range of coatings. The VICOTE Coatings are available through Victrex plc or its preferred coater network. The VICOTE F813Blk grade has been specifically fo..
|
|||