| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 75.0 - 121 °C | 167 - 250 °F | Average value: 111 °C Grade Count:22 |
|
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
|
|||
| Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 87.9 °C Grade Count:4 |
|
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
|
|||
| Drying Temperature | 75.0 - 105 °C | 167 - 221 °F | Average value: 86.1 °C Grade Count:13 |
|
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
|
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
|
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance
Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
|
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance
Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG ..
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
|
LG Chemical NS-161 ABS, Antistatic, High Strength
Information Provided by LG Chem
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
|
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Drying Temperature | 75.0 °C | 167 °F | |
|
Ecomass® 1007TU78 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Polymers
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Star X RF003IU2-BK3047 PA66, Glass Fiber Filled, Impact Modified, Injection Molded
Star X RF003IU2-BK3047 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66/6 Injection Molding (also known as Star X D 1010 14V/3/047)Information provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Staramide A40 PA66, Extrusion
Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar.
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
|
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded
AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
|
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Staramide R1000 PA66, Injection Molded
Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Staramide RB004 PA66, 20% Glass Bead Filled, Injection Molded
Staramide RB004 is a 20% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding
Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Star L PA6 D61 PA6, Injection Molded
Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
|
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded
AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-27 CF30 Polyamide 6 30% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced
50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV2 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, flammability class V2, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning...
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
|
|||
| Drying Temperature |
75.0
-
100
°C <br>@Time 7200 - 14400 sec
|
167
-
212
°F <br>@Time 2.00 - 4.00 hour
|
|
|
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored
High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration..
|
|||
| Drying Temperature |
75.0
-
85.0
°C <br>@Time 14400 - 21600 sec
|
167
-
185
°F <br>@Time 4.00 - 6.00 hour
|
|
|
Eurostar Star L PA6 D83 PA6, Injection Molded
Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
|
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi..
|
|||