| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 2.00 hour | 2.00 hour | |
|
PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
|
|||
| Dry Time | 2.00 hour | 2.00 hour | |
|
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Dry Time | 2.00 hour | 2.00 hour | |
|
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT
(Unverified Data**)
Crastin® LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect, dimensional stability and low warpage and was developed fo..
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
|
|||
| Dry Time | 2.00 hour | 2.00 hour | |
|
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
|
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**)
Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
|
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**)
Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Extrusion Molding |
|
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
|
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
|
LG Chemical HI100K ABS, High Impact
Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion Molding |
|
LG Chemical LI970 Co-Extrusion ASA
Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
|
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
|
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
|
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Dry Time |
2.00
hour <br>@Temperature 80.0 °C
|
2.00
hour <br>@Temperature 176 °F
|
|
|
Lubrizol Advanced Materials Pearlthane® D91T86 Thermoplastic Polyurethane
Type : Pearlthane® D91T86 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties...
|
|||
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
|
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
|
Gromax BTE30-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
|
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..
|
|||
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Extrusion |
|
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Handling |
|
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
|
Pasargad Polymer Peyvand Pasamid 3P-M1130B Nylon 6, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
|
DuPont Performance Polymers Zytel® 70GB30HSL NC010 Nylon 66
Zytel® 70GB30HSL NC010 is a 30% glass bead reinforced heat stabilized polyamide 66 resin.Information provided by DuPont Performance Polymers
|
|||
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
|
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
(Unverified Data**)
Zytel® RS 30G30L NC010 is a lubricated, 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewably sourced ingredients by weight (60% based on polymer only). It was initia..
|
|||
| Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
|
Gromax CFG33-QS11N1 Nylon 6 33% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||