| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
PolyOne OnFlex™ BIO 5380A-E0006 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F.
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled
CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F.
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||