| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
|
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE)
Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora..
|
|||
| Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
|
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)
The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
|
|||
| Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
|
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.000 - 0.552 MPa | 0.000 - 80.1 psi | |
|
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE)
Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat ..
|
|||
| Back Pressure | 0.000 - 0.758 MPa | 0.000 - 110 psi | |
|
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV..
|
|||
| Back Pressure | 0.000 - 0.827 MPa | 0.000 - 120 psi | |
|
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
|
|||
| Back Pressure | 0.000 MPa | 0.000 psi | |
|
Nanocyl PLASTICYL™ PA1501 Polyamide 66 with 3 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
|
|||
| Back Pressure | 0.000 - 1.03 MPa | 0.000 - 149 psi | |
|
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
|
|||
| Back Pressure | 0.000 - 1.03 MPa | 0.000 - 149 psi | |
|
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
|
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
|
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
|
|||
| Back Pressure | 0.000 - 10.0 MPa | 0.000 - 1450 psi | |
|
Kingfa LONOY 1300 PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
|
|||
| Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
|
LG Chemical LUCEL HI-525 High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
|
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
|
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
|
|||
| Back Pressure | 0.000 - 3.92 MPa | 0.000 - 569 psi | |
|
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
|
Gromax PBT 1100-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
|
|||
| Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
|
MRC Polymers EMAREXâ„¢ 400 GF33 Nylon 6/6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
|
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.000 - 0.345 MPa | 0.000 - 50.0 psi | |
|
Clariant Renol 66G33-L Nylon 66, 33% Glass Fiber Reinforced, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
 
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
|
|||
| Back Pressure | 0.000 - 0.300 MPa | 0.000 - 43.5 psi | |
|
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
|
|||