| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass
Information provided by Star Plastics, Inc.
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP 1061 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP 1249B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1488A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1586UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1679L2 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2100 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2241 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2242 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2253 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2287 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2676 UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2740UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® OBC 4560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-1377A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-1524F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-3260-1 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-90-T3030A-80 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
|
|||
| Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
|
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-87-L832-E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
|
Teknor Apex Uniprene® UN-7100-40D Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2854T Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2890M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2750 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 24.9 - 50.0 psi | |
|
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **)
Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 24.9 - 50.0 psi | |
|
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)
Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr..
|
|||