Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Back Pressure = 0.300 MPa Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 1100-211X
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 1100-630S
Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1100-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 3030-201 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 4115-104D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 4130-201D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 DB Thermoplastic Polyurethane
Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports foo..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 DE Thermoplastic Polyurethane
Introduction: AVALON 65 DE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DE is part of the AVALON Perform Range and offers a premium soling material for sports foo..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane
Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 70 AE Thermoplastic Polyurethane
Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material ..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 75 AE Thermoplastic Polyurethane
Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material ..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 85 ABX Thermoplastic Polyurethane
Introduction: AVALON 85 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABX is part of the AVALON Perform Range and offers a specially designed,..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 85 AE Thermoplastic Polyurethane
Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 92 AE Thermoplastic Polyurethane
Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 1100-104S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 1100-600S
Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 2000-104D
Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 2000-201D
Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 2100-104B
Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1100-211MB
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1200-211D
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Copyright © lookpolymers.com All Rights Reserved