| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
|
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
NatureWorks® Ingeo™ 3001D Injection Grade PLA
NatureWorks® PLA (polylactide) polymer 3001D is designed for injection molding applications. It is designed for clear applications with heat deflection temperatures lower than 130ºF (55ºC). Appli..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
NatureWorks® Ingeo™ 3251D Injection Grade PLA
IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow..
|
|||
| Back Pressure | 0.0689 - 0.689 MPa | 10.0 - 100 psi | |
|
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **)
Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**)
Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi..
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
|
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
|
|||
| Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi | |
|
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced
Information provided by FIBERFIL Engineered Plastics
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
Star Plastics PC1510R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1486A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1775 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2100-S-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2241 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2775 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer
A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
|
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
|
Diamond Polymers ASA/PC FA-30
Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc.
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2691A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2730B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | Processing |
|
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for..
|
|||