Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Back Pressure = 43.5 psi Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed,..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 80 ABX Thermoplastic Polyurethane
Introduction: AVALON 80 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABX is part of the AVALON Perform Range and offers a specially designed,..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 98 AB Thermoplastic Polyurethane
Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 1100-630S
Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PET 9130-104 30% Glass Filled
Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1100-211S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 4140-201D 40% Glass Fiber Filled
Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 5130-104 30% Glass Fiber Filled
CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane
Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 AC Thermoplastic Polyurethane
Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 AE Thermoplastic Polyurethane
Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 DE Thermoplastic Polyurethane
Introduction: AVALON 65 DE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DE is part of the AVALON Perform Range and offers a premium soling material for sports foo..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane
Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 75 AE Thermoplastic Polyurethane
Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material ..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 92 AE Thermoplastic Polyurethane
Introduction: AVALON 92 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 92 AE is part of the AVALON Perform Range and offers a premium soiling materi..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 95 AEU Thermoplastic Polyurethane
Introduction: AVALON 95 AEU is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AEU is part of the AVALON Perform Range and offers a premium soiling mate..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1100-211XG
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1200-211L
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 3020-104 15% Glass Fiber Filled
Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 3030-104 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 1200-211E
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 6730-104F Glass/Mineral Filled
Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1200-211D
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 4115-201D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Back Pressure 0.000 - 0.300 MPa
0.000 - 43.5 psi
Gromax PBT 1200-211M
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..