| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Vyram™ 9101-55 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Vyram™ 9203-54 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
|
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
|
Kingfa FRHIPS-1162 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl..
|
|||
| Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
|
Kingfa FRHIPS-220 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica..
|
|||
| Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
|
Kingfa FRHIPS-8002 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec..
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3020X8 Nylon 12 Thermister
Description: UBESTA Nylon 12 ThermisterInformation provided by UBE.
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U..
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE.
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE.
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3035LU1 Rigid Piping Grade Nylon 12
Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Back Pressure | 5.00 - 10.0 MPa | 725 - 1450 psi | |
|
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Back Pressure | 5.00 - 10.0 MPa | 725 - 1450 psi | |
|
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
|
|||
| Back Pressure | 5.00 - 10.0 MPa | 725 - 1450 psi | |
|
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Back Pressure | 5.00 - 15.0 MPa | 725 - 2180 psi | |
|
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Back Pressure | 5.00 MPa | 725 psi | Injection Molding |
|
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE.
|
|||
| Back Pressure | 5.00 - 20.0 MPa | 725 - 2900 psi | Extrusion |
|
ExxonMobil Santoprene® 241-73 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
|
|||