| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem DIOSHY® GP-935-UB2 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem DIOSHY® MP-960NC TPE Compound
This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem GP-975 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem HP-930NC-HD TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem MP-850 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem SE/PA745B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Stellarchem SV-B87E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
|
|||
| Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
|
Teknor Apex Beetle® MDF50 Nylon 6, 50% Short Glass Fiber Filler
Notes: MDF50 is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish Features: Good Surface FinishProcessing Method: Injection molding F..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Teknor Apex Sarlink® 4180 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4180 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Teknor Apex Sarlink® 4390 Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4390 is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Teknor Apex Sarlink® 4480 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4480 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
|
|||
| Screw Speed | 160 - 200 rpm | 160 - 200 rpm | |
|
Lubrizol Estane® T365A Thermoplastic Polyurethane
Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor..
|
|||
| Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
|
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer
A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
|
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
|
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
|
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection |
|
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 60 - 200 rpm | 60 - 200 rpm | Injection |
|
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | Injection Molding |
|
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer
A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set ..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Screw Speed | 100 - 200 rpm | 100 - 200 rpm | |
|
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..
|
|||