Polymer Property : Screw Speed = 200 rpm Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber  (discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem AB870EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem GP-915UB TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem GP-9401 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem MP-850 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Stellarchem SV-B65E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Screw Speed 160 - 200 rpm
160 - 200 rpm
Lubrizol Estane® T460A Thermoplastic Polyurethane
Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer
A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer
Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer
Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 60 - 200 rpm
60 - 200 rpm
Injection
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Teknor Apex Sarlink® 3480 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Screw Speed 100 - 200 rpm
100 - 200 rpm
Injection Molding
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl..
Screw Speed 100 - 200 rpm
100 - 200 rpm
ExxonMobil Santoprene® 241-45 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water. This grade ..