Polymer Property : Screw Speed = 30 rpm Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Screw Speed 30 - 50 rpm
30 - 50 rpm
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Screw Speed 30 - 50 rpm
30 - 50 rpm
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc.
Screw Speed 30 - 50 rpm
30 - 50 rpm
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
Screw Speed 30 - 50 rpm
30 - 50 rpm
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom..
Screw Speed 30 - 60 rpm
30 - 60 rpm
Nilit Polynil® N66-P50N Lubed Nylon 6/6
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Screw Speed 30 - 60 rpm
30 - 60 rpm
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical HIPS 405AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL GP2200 PP+GF20%
Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL GP3200 PP+MF20%
Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL HI5204 PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow
Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica..
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL LW4302 PP+GF/MF30%
Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Screw Speed 30 - 120 rpm
30 - 120 rpm
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Screw Speed 30 - 120 rpm
30 - 120 rpm
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Screw Speed 30 - 120 rpm
30 - 120 rpm
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Screw Speed 30 - 120 rpm
30 - 120 rpm
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Screw Speed 30 - 120 rpm
30 - 120 rpm
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Screw Speed 30 - 150 rpm
30 - 150 rpm
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Screw Speed 30 - 80 rpm
30 - 80 rpm
Extrusion
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Screw Speed 30 - 50 rpm
30 - 50 rpm
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
Screw Speed 30 - 50 rpm
30 - 50 rpm
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding
LG Chemical LUPOL GP3100 PP+MF10%
Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Screw Speed 30 - 75 rpm
30 - 75 rpm
LTL Color Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy
V-0 rated polycarbonate-ABS alloy, excellent toughness and light stabilityAll information provided by LTL Color Compounders, Inc.
Screw Speed 30 - 80 rpm
30 - 80 rpm
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant
Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang