| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm | |
|
Multibase Multi-Pro® 1008 T Polypropylene
Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm | |
|
Multibase Multi-Pro® 4010 M Polypropylene
Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 40 - 80 rpm | 40 - 80 rpm | |
|
PTS Trimid® N6-200L Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
|
Ravago Manufacturing Americas Hylon® N1033STL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Screw Speed | 40 - 80 rpm | 40 - 80 rpm | |
|
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6
Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
|
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM)
Information provided by Ravago.
|
|||
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm | |
|
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
|
|||
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm | |
|
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
|
|||
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm | |
|
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
|
|||
| Screw Speed | 40 - 100 rpm | 40 - 100 rpm | |
|
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
|
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6
(discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
|
|||
| Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
|
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Screw Speed | 40 - 75 rpm | 40 - 75 rpm | Injection Molding |
|
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity
Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Screw Speed | 40 - 75 rpm | 40 - 75 rpm | Injection Molding |
|
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity
Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
|
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
|
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded
V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
|
LG Chemical Lupox® GP-2151F General Purpose PBT, 15% Glass Fiber Reinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Screw Speed | 40 - 75 rpm | 40 - 75 rpm | |
|
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |
|
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
|
|||
| Screw Speed | 40 rpm | 40 rpm | |
|
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
|
|||
| Screw Speed | 40 rpm | 40 rpm | |
|
Multibase Multi-Flex® A 7025 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
|
|||
| Screw Speed | 40 rpm | 40 rpm | |
|
Multibase Multi-Flex® A 7101 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
|
|||
| Screw Speed | 40 rpm | 40 rpm | |
|
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
|
|||
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded
V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc.
|
|||