| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
|
|||
| Screw Speed | 50 - 150 rpm | 50 - 150 rpm | |
|
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV..
|
|||
| Screw Speed | 50 - 90 rpm | 50 - 90 rpm | |
|
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**)
Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**)
Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | Injection Molding |
|
LG Chemical LUCEL HI510 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Screw Speed | 50 rpm | 50 rpm | |
|
Lubrizol Advanced Materials PEARLTHANE® D16N98UV Thermoplastic Polyurethane Elastomer
Pearlthane® D16N98UV is a polyether-based TPU, supplied in form of transparent, colorless pellets, combining high hardness with excellent mechanical properties and good hydrolysis and microbial r..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | Injection Molding |
|
LG Chemical ER461 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
|
|||
| Screw Speed | 50 - 200 rpm | 50 - 200 rpm | |
|
Teknor Apex Beetle® MDM54 Nylon 6, Non-halogenated, Mineral Reinforced
Notes: MDM54 is a UL recognized, V-2 rated halogen and phosphorus-free flam retarded, mineral filled injection molding grade of nylon 6, primarily intended for electrical applications; U.L. 94 V-2 a..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Monprene® MP-1564F Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Monprene® MP-1662-L1 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Monprene® MP-2336UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Monprene® MP-2755 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL EF-6155 UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2448G Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2478K Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2540A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2570A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2625A Thermoplastic Elastomer
Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2635B Thermoplastic Elastomer
Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-3954-50 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-6055 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-81-D965-P Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-90-T3030A-80 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
|
|||
| Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
|
Teknor Apex Uniprene® UN-1674C Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
|
|||
| Screw Speed | 50 - 60 rpm | 50 - 60 rpm | |
|
TPI Porene® ABS-AN450 Flame Retardant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-2580A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
|
Teknor Apex Uniprene® UN-7100-73 Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..
|
|||
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | |
|
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||